ارسل ملاحظاتك

ارسل ملاحظاتك لنا







Study the Mineralogy of Al-Faw Soil in Southern Iraq and Determine Swelling Properties by Indirect Methods

المصدر: مجلة ميسان للدراسات الأكاديمية
الناشر: جامعة ميسان - كلية التربية الأساسية
المؤلف الرئيسي: Abdalamer, Haneen N. (Author)
مؤلفين آخرين: Daham, Huda A. (Co-Author)
المجلد/العدد: مج23, ع49
محكمة: نعم
الدولة: العراق
التاريخ الميلادي: 2024
الشهر: آذار
الصفحات: 174 - 183
DOI: 10.54633/2333-023-049-018
ISSN: 1994-697X
رقم MD: 1458258
نوع المحتوى: بحوث ومقالات
اللغة: الإنجليزية
قواعد المعلومات: EduSearch, HumanIndex
مواضيع:
كلمات المؤلف المفتاحية:
Clay Minerals | Swelling Soil | X-Ray Diffraction | Plasticity Index | Clay High Plasticity
رابط المحتوى:
صورة الغلاف QR قانون
حفظ في:
LEADER 02657nam a22002537a 4500
001 2203500
024 |3 10.54633/2333-023-049-018 
041 |a eng 
044 |b العراق 
100 |9 772725  |a Abdalamer, Haneen N.  |e Author 
245 |a Study the Mineralogy of Al-Faw Soil in Southern Iraq and Determine Swelling Properties by Indirect Methods 
260 |b جامعة ميسان - كلية التربية الأساسية  |c 2024  |g آذار 
300 |a 174 - 183 
336 |a بحوث ومقالات  |b Article 
520 |b This study aims to determine the capacity of surface soils, the loading layers of engineered structures with shallow foundations, to swell. For this, five samples were collected using a hand auger at a depth of 1.5–2 meters in the city of Al-Faw in Basra, Iraq. The swelling potential of the soils in the research area was calculated using the clay content, liquid limit, plasticity index, and shrinkage limit values, and the constituent minerals were identified using X-ray diffraction. According to the results of the Atterberg’s limit tests, the soil samples taken from the city of Al-Faw fall into one of three categories: clayey silt low plasticity (ML), clay high plasticity (CH), or silty clay low plasticity (CL). The liquid limit in soil samples ranges between 34-55%, and the plasticity index values range between 12 and 28%. Three samples are of medium swelling potential, while the third location has high swelling potential and the second location has low swelling potential, and the X-ray diffraction data demonstrate that Montmorillonite is the main dominant clay mineral, accounting for an average of 31.88%, followed by Kaolinite mineral, which accounts for an average of 28.984%, Illite, which accounts for an average of 19.5702%, Chlorite, which accounts for an average of 12.1864%, and Palegorskite, which accounts for an average of 7.3688%. 
653 |a المعادن الطينية  |a خواص التربة  |a التربة المنتفخة  |a العراق 
692 |b Clay Minerals  |b Swelling Soil  |b X-Ray Diffraction  |b Plasticity Index  |b Clay High Plasticity 
700 |9 772724  |a Daham, Huda A.  |e Co-Author 
773 |4 التربية والتعليم  |4 العلوم الإنسانية ، متعددة التخصصات  |6 Education & Educational Research  |6 Humanities, Multidisciplinary  |c 018  |e Maisan Journal of Academic Studies  |f Maǧallaẗ Mīsān li-l-dirāsāt al-akādīmiyyaẗ  |l 049  |m مج23, ع49  |o 2333  |s مجلة ميسان للدراسات الأكاديمية  |v 023  |x 1994-697X 
856 |u 2333-023-049-018.pdf 
930 |d y  |p y  |q y 
995 |a EduSearch 
995 |a HumanIndex 
999 |c 1458258  |d 1458258 

عناصر مشابهة